Ayyukan Jiyya na Zafi a Kasuwan Ƙarfe na Ƙarfe: Quenching, Tempering, Normalizing da Annealing na Karfe
Maganin zafi muhimmin mataki ne na tabbatar da ingancin kayan aikin sassan ƙarfe na siminti. Ta hanyar ƙirƙira, zubawa, girgizawa da tsaftacewa, simintin yana ɗaukar siffarsa ta ƙarshe - amma ƙila ba zai yi ƙarfi ko sassauƙa ba don amfani na ƙarshe. Ta hanyar dumama da sanyaya ƙarfe a farashi daban-daban, masana'antun ƙarfe na iya canza halayen injinan su. Amma ta yaya amfani da zafi ke canza ƙarfi ko sassaucin ƙarfe ?
Crystallization da Metal Properties
Lokacin da narkakkar ƙarfe ya huce, yana ƙarfafawa ya zama tsarin crystalline. Ƙarƙashin na'urar hangen nesa, waɗannan sifofin sun yi kama da yanayin sanyi da ke tasowa akan gilashi a lokacin hunturu. Kowane tsari yana girma daga tsakiya har sai ya hadu da wani tsarin crystal. Wadannan sifofi sun hada da "hatsi" na karfe.
Kamar yadda yanayin hunturu daban-daban ke samar da nau'ikan yanayin sanyi iri-iri, yanayin zafi daban-daban kuma yana canza lu'ulu'u da aka samu yayin yin ƙarfe. Hatsin da suke samarwa yawanci ba a iya gani amma suna bayyana lokacin da ƙarfe ya cika da acid.
Siffai da alaƙar hatsi a cikin gami suna ƙayyade kaddarorin injin sa. Lokacin da aka bugi ƙarfe, zagayawar hatsi na iya zamewa da juna, haɗewa maimakon tsayayye ko karyewa. Lebur hatsi na iya tarawa kamar bulo a bango kuma su goyi bayan juna; sun fi karfi fiye da hatsi mai zagaye amma har yanzu suna ba da izinin motsi. Jagged, cuku-cuku masu tsaka-tsaki na iya ba da kyauta kwata-kwata. Maganin zafi na karafa na iya sake fasalin crystallization, ta yadda za su canza hatsinsu kuma ta haka ne kaddarorin karfe.
Karfe masu taurin aiki
Hoton maƙerin da ke buga farantin ƙarfe mai ƙyalli a cikin ƙirjin sa, duk da cewa ba kowa ba ne, nan take ake gane shi. Koyaya, ga mafi yawan tarihin ɗan adam, maƙera suna yin aikin ƙarfe da injina don ƙara ƙarfi. A yau, maƙera ba sa yin ƙirƙira da hannu da ƙarfe amma galibi ana birgima don taurare shi.
Hoton tsarin hatsi yana bayyana tasirin taurin aiki. Zagayewar da ke cikin ƙarfen nakasar, da sabbin sifofinsu suna ba da ƙarfin ƙarfe. Misali, a cikin jujjuyawar sanyi, ana matse hatsin da ke zagaye da shimfiɗa, suna zama kamar sanduna. Waɗannan sanduna suna tallafawa juna, kamar tarin sanduna. Maƙera ko mai aikin ƙarfe na iya yin guduma, murɗawa, zafi, sanyi, da shimfiɗa abu don canza siffar hatsi. Idan hatsi ba su da inda za su je lokacin da aka buge su, sun samar da matrix inelastic matrix, wanda hakan zai kara taurin karfe.
Duk da haka, wannan taurin na iya zuwa da tsada: ƙarfi na iya sa kayan ya lalace. Hatsi masu siffa ba bisa ƙa'ida ba ba sa zamewa da juna cikin sauƙi: an haɗa su tare. Duk wani tasiri mai girma isa - mafi girma fiye da ƙarfin haɗin tsakanin hatsi - zai raba su.
Karfe masu zafi
Kamfanoni sun fara ƙirƙirar kayan aikin injiniyan da ake so na karfe ta hanyar zabar gami da aka sani don samar da waɗannan halaye. Duk da haka, yayin da simintin gyare-gyaren ya yi sanyi, ƙirƙira na wannan ƙarfe ya kusan yiwuwa a sarrafa shi. Tun da crystallization yana rinjayar injiniyoyin ƙarfe, gami ba zai iya yin aiki da kyau ba sai an ƙara sarrafa shi. Kamfanonin kafa za su iya cimma wannan ta hanyar dumama da sanyaya ƙarfe a cikin tsari da tsari na yau da kullun.
Maganin zafi hanya ce mara lalacewa ta canza kaddarorin kayan. Wani lokaci tsari ne na biyu na karafa masu taurin aiki - amma ita ce hanyar da aka fi so don wuraren da aka kafa domin simintin gyare-gyaren sun riga sun kasance daidai kuma ba za a iya sarrafa su ba.
Crystallization kusan koyaushe yana farawa daga saman waje kuma yana motsawa zuwa ciki, kuma - musamman a cikin manyan simintin gyare-gyare - akwai babban bambancin zafin jiki tsakanin harsashi da tsakiyar simintin. Lu'ulu'u suna girma ba bisa ka'ida ba, yawanci suna zama masu kaifi da ƙarancin ductile kusa da saman. Yawancin lokaci sun fi zagaye, kuma don haka suna da laushi yayin da suke tafiya. Siffar simintin gyare-gyare da lahani ko haɗawa a cikin ƙarfe na iya rinjayar ƙimar sanyaya, haifar da kaddarorin inji daban-daban a wurare daban-daban na ƙarfe. Wadannan bambance-bambance na iya haifar da nau'in karfe na ciki, wanda zai haifar da gajiyar karfe ko gazawa. Maganin zafi yana ba wa masana'antun damar komawa cikin ƙarfe kuma su sake tsara lu'ulu'u waɗanda ke yin sa.
Soaking shine tsarin kawo simintin gyare-gyare sama da wurin sake sakewa. Ƙayyadaddun "lokacin zafi" don jiƙa a cikin maganin zafi yana ba da damar lu'ulu'u a cikin karfe don narke da sake tsarawa. Yin bita da zagayowar lokaci na ƙarfe-carbon zai iya taimaka wa masana'antun su fahimci tsawon lokacin da za a ci gaba da yin simintin gyare-gyare a wani yanayin zafi don ba da damar takamaiman yaduwar carbon.
A mafi yawancin (amma ba duka) sassan zagaye na ƙarfe-carbon lokaci ba, jiƙan simintin gyare-gyare ko sarrafa karafa yana rage taurinsu da gaɓoɓinsu. Yayin da barbashi a cikin karfe ke girma akai-akai, suna zama zagaye kuma suna iya sake tsarawa akan tasiri ta zamewa da juna. Bugu da ƙari, tunda abu koyaushe yakan kai yanayin zafi ɗaya, lu'ulu'u yawanci sun fi na waɗanda ke cikin sabbin simintin gyare-gyare.
Ƙullawa
Annealing yana farawa da jiƙa kuma yana ci gaba ta sannu a hankali sanyaya ƙarfe a cikin tanderun. Wanda ya samo asali yana kashe tanderun kuma yana ba da damar zafin jiki ya ragu a hankali da sarrafawa. A lokacin dumama da sanyaya, dukan abu yana da daidaito na thermal, wanda ke nufin akwai ƙananan damuwa na ciki: ba za a sami "yankuna" na karfe tare da kaddarorin crystalline daban-daban ba. Karafa da aka toshe galibi suna da kyakykyawan ductility, tare da karuwar ductility, karfin juriya da tsawo. Saboda jinkirin sanyaya lankwasa, girman hatsin karafa da aka toshe yawanci babba ne.
Daidaitawa
Daidaita ƙarfe ya haɗa da dumama shi zuwa zafin jiki na recrystallization sannan a fitar da shi daga cikin tanderun da sanyaya shi a cikin yanayi. Yawancin kaddarorin ƙarfen da aka cire su ma suna kasancewa a cikin ƙarfe na al'ada, amma saboda rashin cikar yanayin sanyaya, hatsi galibi ba su da yawa. Duk da haka, bambancin zafin jiki ya yi ƙasa da na a cikin ƙarfe mai sanyi, wanda ke nufin cewa daidaitattun samfuran ba su da ƙarfi.
Yawan sanyaya da ake samu a cikin daidaitawa yana samar da ƙananan hatsi a cikin ƙarfe fiye da annealing, wanda ke nufin cewa yawanci ya fi karfi ko wuya fiye da karfen da aka shafe.
Irƙwara
Me zai faru idan ana buƙatar taurin gaske? A cikin kera kayan aiki da sassan injin, tausasa ƙarfe na iya karya manufar.
Maganin zafi na iya ba da izini ga ƙayyadaddun ƙayyadaddun taurin kai. Don yin ƙarfe mai ƙarfi, masana'antun suna nutsar da ƙarfen har sai austenite ya zama mafi girman ƙwayar cuta sannan kuma a kashe shi cikin mai sanyi ko iska mai ƙarfi. Lokacin da austenite ya kasance cikin girgiza mai sanyi, yana samar da wani tsari mara kyau na crystal wanda ake kira martensite. Saboda lalacewar carbon a cikin kowane kwayoyin martensite, wannan abu ya fi wuya.
Tun da quenching yana faruwa daga waje a ciki, manyan abubuwa suna ƙarƙashin matsin lamba na saurin crystallization, wanda zai iya haifar da damuwa na ciki a cikin karfe. Idan quenching ya wuce gona da iri, waɗannan dakarun na iya haifar da tsagewa wani lokaci. Saboda haka, kashe ruwa ba ya zama ruwan dare ga manyan abubuwa na karfe saboda yana haifar da raguwar zafin jiki da sauri, yana haifar da fashewa. Man fetur da iska sun yi sanyi kaɗan da ƙarfi.
Koyaya, quenching yana taurare fiye da ƙarfe kawai. Ana amfani da quenching na ruwa a wuraren da aka samo asali. Ƙarfe ɗin da ba ƙarfe ba maiyuwa ba za su iya jure matsi iri ɗaya ba saboda matakan su da tsarin kwayoyin halitta sun bambanta. Manganese za a iya kashe ruwa a yanayin zafi mafi girma fiye da karfe ba tare da tsagewa ba. Koyaya, bambancin zafin jiki yana da girma sosai cewa kowane quenching zai iya ɗaukar adadin kuzari mai yawa wanda zai iya yin kuskure! A ƙasa akwai fashewa yayin aikin kashe simintin ƙarfe na manganese wanda ya haifar da ragowar yashi.
Jin zafi
Ana iya samun daidaitattun ma'auni na taurin da ductility ta hanyar tsari da ake kira tempering. Yawancin lokaci ana yin zafi akan karfen da aka kashe don sanya shi ya ragu yayin da yake riƙe da ɗan tauri. A cikin zafin rai, ƙarfen yana sake zafi, amma a yanayin zafi ƙasa da wanda ake amfani da shi wajen kashewa, daidaitawa, ko kashewa.
Martensite ba tsarin kwayoyin halitta bane mai ƙarfi a yanayin zafi mai yawa - yana samuwa a ƙarƙashin girgiza - don haka ƙarfe mai zafi yana nufin sanya martensite ya zama mara ƙarfi kuma yana sa shi ya fara canzawa zuwa siminti da ferrite. Matsakaicin zafin jiki da tsawon lokacin da ke cikin tanderun dumama zai shafi girman canjin martensite, don haka laushin ƙarfe. Misali, ana iya rage maɓuɓɓugan ƙarfe a yanayin zafi mai girma don ƙara laushi idan aka kwatanta da kayan aikin da aka rage zafi a yanayin zafi mai ƙasa don kiyaye tauri.
Ana amfani da zafin jiki sau da yawa don rage damuwa na ciki a cikin kayan da aka kashe. Ƙarfe wanda ya fuskanci wasu matsalolin zafi, kamar walda ko ƙirƙira, ana iya yin zafi don ƙyale ƙwayoyin ciki su ɗan ɗan sassauta.
Bambance-bambancen maganin zafi
A cikin kafuwar, simintin gyare-gyare yawanci ana yin maganin zafi iri ɗaya. Koyaya, wasu lokuta abubuwa na iya fuskantar maganin zafi na yau da kullun. Takubban ƙarfe masu zafin rai yawanci suna fuskantar digiri daban-daban na zafin jiki don yin ƙarfi yayin da suke kiyaye ainihin roba. Maɓuɓɓugar ruwa wani lokaci suna shan magunguna daban-daban na zafi don dacewa da ayyukansu.
Vigor yana da fiye da shekaru 18 na gwaninta a fannin sarrafa zafi na siminti, kayan ƙarfe da sauran sassan ƙarfe . Idan kuna da wata tambaya da buƙata game da haɓaka samfura ko inganta sarkar samar da kayayyaki, da fatan za ku iya tuntuɓar mu a info@castings-forging.com